Увођење

Closure makers searching “8011 lacquered aluminum for bottle caps price” need a thin, food-safe, pre-coated aluminum strip that runs on high-speed cap presses to make ROPP wine and spirit closures, screw caps and pharmaceutical seals.

8011 is an aluminum-iron alloy with the formability, low earing and pinhole-free surface these operations demand, and “lacquered” means it arrives already coated inside and out.

Buying lacquered coil rather than bare stock removes an in-house coating step and guarantees a cured, compliant food-contact surface.

This guide covers the standard gauges and tempers, the lacquer systems and compliance, како се гради цена, indicative ranges and exactly what to specify for an accurate quotation.

Lacquered 8011 cap-stock coils, ready for the press.
Lacquered 8011 cap-stock coils, ready for the press.

Шта је 8011 Lacquered Cap Stock?

8011 is a non-heat-treatable 8xxx-series alloy with about 0.6–1.0% iron and 0.5–0.9% silicon; it is strengthened by cold rolling. For closures it is supplied two ways:

  • Bare (mill) coil—uncoated strip for converters who apply their own lacquer and print.
  • Lacquered coil—pre-coated strip with a food-grade internal coating and a colored, gold or clear external coating, sometimes printed, ready to stamp.

Alloy alternatives are 8011A, 3105, 1200 и 1100, али 8011 is preferred where low pinholes, good deep drawing and a low earing rate matter.

Note that crown corks (beer bottle caps) are normally tinplate/ECCS, not aluminum, and should not be confused with aluminum ROPP and screw closures.

Standard Gauges, Tempers and Tolerances

Параметар Типичан опсег за 8011 капа залиха
Нарав Х14, Х16, Х24, Х26 (H18/H19 for stiffer or harder caps)
Дебљина about 0.16–0.23 mm (уобичајено 0.17, 0.20, 0.22 мм)
Ширина about 50–900 mm slit strip (wider coil on request)
Толеранција дебљине about ±0.005 mm
Earing rate typically ≤2% to limit press scrap
Пинхолес 0 по м²; surface free of oil, roll marks and stains
Цоре / packing 76 мм или 152 мм ИД; about 38–42 kg per roll, wooden cases

 

Tensile strength is roughly 110–155 MPa across H14–H16 with the elongation needed for rolling and embossing; exact values depend on gauge and should be agreed on the MTC.

Harder tempers hold thread and tamper bands, while softer ones draw more deeply.

Internal and External Lacquer Systems

The internal (product-contact) coating protects the metal and contents and is the most carefully specified; the external coating carries color, print and corrosion protection.

  • Internal: epoxy-phenolic / epoxy-polyamino remains mainstream for strong adhesion and resistance to acid, oil and heat; polyester and water-based systems are also used.
  • BPA-NI: coatings made without intentionally adding BPA, BADGE or BFDGE; BPA-NI is a formulation claim, so confirm the actual polymer system and migration records.
  • External: злато, colored or clear baking lacquer or print primer.
  • Film build: about 12–18 μm dry on the face and 5–8 μm on the back, depending on the cap.

Coating quality is verified by cross-cut adhesion (разреда 0), 0T bend without cracking or peeling, MEK rub resistance, heat resistance and, where required, an HgCl₂ test; the film must survive drawing, thread rolling and embossing without flaking.

Cap strip being lacquered and cured on a coil coating line.
Cap strip being lacquered and cured on a coil coating line.

Food-Contact Compliance

Closure stock is supplied to the market’s food-contact rules—FDA 21 CFR in the US, the EU framework including Regulation (ЕУ) 10/2011,

LFGB in Germany and GB 4806 in China—with overall and specific migration, and heavy-metal limits, documented per coating and gauge.

Ask for the declaration of compliance, migration test reports and, for BPA-NI, a written statement; market trends also move toward PVC-free and PFAS-free packaging coatings.

Coating choice also depends on the contents and filling process. Wine and oil are relatively forgiving, whereas carbonated drinks, juice and vinegar are more aggressive and need an internal lacquer proven for that pH, with the liner and bottle

checked together; hot-fill or pasteurised lines require heat resistance and the cap must hold seal pressure over shelf life.

Matching the lacquer to the product up front avoids corrosion spots, off-taste or leaks that a generic food-grade label alone does not prevent.

Главне апликације

  • РУДЕ (roll-on pilfer-proof) closures for wine, духови, olive oil and bottled water.
  • Aluminum screw caps for beverages, oils and general bottled products.
  • Pharmaceutical vial seals and flip-off / PP caps, plus cosmetic and personal-care closures.
  • Tamper-evident and perforated break-band caps, printed or embossed to brand.
Finished aluminum ROPP and screw closures on bottles.
Finished aluminum ROPP and screw closures on bottles.

How the Price Is Built and Indicative Ranges

Bare 8011 coil is priced per metric ton as the aluminum ingot base plus a rolling fee. Lacquered coil adds the coating material (internal and external), coil coating and curing, printing if required, plus inspection, so it is quoted per ton of finished strip and costs more than bare stock.

Because the ingot component moves daily with LME/Shanghai prices and the coating system varies, no fixed annual price is possible.

Форма производа Indicative B2B reference (ФОБ, по тони)
Bare 8011/3105 cap coil roughly the ingot price plus a rolling fee (commonly in the low-thousands US$/MT)
Lacquered / coated closure coil about US$2,200–3,500/MT in common listings, varying with gauge and coating
Штампано / multi-color or BPA-NI coil higher again, depending on colors and compliance package

 

These are indicative platform ranges, није фиксна понуда; reconfirm against today’s ingot price, мерач, ширина, coating and quantity, and compare like-for-like on the same Incoterm.

Lacquered 8011 strip running on a high-speed cap press.
Lacquered 8011 strip running on a high-speed cap press.

Quality Control and How to Order

За прецизну цену, послати: легура и темперамент (8011 Х14/Х16); дебљина и толеранција; slit width; bare or lacquered; internal coating (epoxy/polyester/BPA-NI) and external color or print; dry film build; цоре ИД;

тежина ролне; количина; target market and compliance (FDA/LFGB/EU/GB); packing and destination port. QC covers gauge, ширина, минђуша, рупице, површине, adhesion and migration on certificates,

with ISO 9001 and SGS/BV inspection available. Verify new material on production-gauge samples run at normal press speed, and use a signed sample as the receiving standard. Common terms are 30% deposit, balance against the bill of lading, FOB/CFR/CIF.

Confirm the supplier genuinely rolls and coats in-house rather than reselling spot strip: only an integrated line can hold gauge, color and coating weight across lots and re-supply the same specification.

Audit the coating line, request samples from the target gauge and color, run them on your press and with your contents, and approve a signed sample before bulk.

Често постављана питања

П: What is the price of 8011 лакирани алуминијум за чепове боца?

А: It is quoted per ton of finished strip as the ingot and rolling cost plus the internal/external coating; common B2B listings sit roughly between about US$2,200 and 3,500/MT FOB depending on gauge and coating, with printed or BPA-NI higher. Request a same-day quote.

П: Why buy lacquered coil instead of bare coil?

А: Lacquered strip is already coated and cured with a compliant food-contact surface, removing an in-house coating step; bare coil only suits converters with their own coating line.

П: Which gauge and temper are standard?

А: About 0.16–0.23 mm (често 0.17/0.20/0.22 мм) in H14 or H16, slit to the press width with a low earing rate and zero pinholes.

П: Is the coating BPA-NI and food safe?

А: BPA-NI, епокси, polyester and water-based internal coatings are available with FDA, ЛФГБ, EU and GB migration documentation; BPA-NI is a formulation claim, so request the polymer details.

П: Can it make beer crown corks?

А: No—crown corks are normally tinplate/ECCS. This aluminum strip makes ROPP, screw, pharmaceutical and cosmetic closures.

П: Шта је МОК и време испоруке?

А: MOQ is commonly about 1–3 tons per specification with samples and trial orders available; време испоруке зависи од мерача, премазивање, printing and quantity.

Закључак

8011 lacquered cap stock is the ready-to-press, food-safe aluminum strip behind ROPP, screw and pharmaceutical closures.

Its price combines the aluminum market with the coating system, so define the temper, мерач, ширина, internal and external lacquers and compliance, then compare like-for-like per ton on the same Incoterm and approve production samples before bulk.