The pamungkas Guide to 3003 Lambaran Aluminium pikeun Aplikasi Gambar Jero: Naha Ngadominasi Industri Cookware sareng Tekanan Kapal
In the world of metal fabrication, specifically within the gambar jero séktor, selecting the right alloy is the difference between a high-quality finished product and a pile of scrap metal. While many aluminum alloys exist, éta 3003 alumunium Sepré has emerged as the industry standard for manufacturers of cookware, kapal tekanan, and fuel tanks.
This comprehensive guide explores the unique properties of 3003 alumunium, its technical advantages in deep drawing, and a critical comparison with other alloys, backed by real-world factory case studies.

1. What Makes 3003 Aluminum Sheet the King of Deep Drawing?
Deep drawing is a manufacturing process where a sheet metal blank is radially drawn into a forming die by the mechanical action of a punch. For this to succeed without cracking or “orange peel” defects, the metal must possess exceptional digana jeung work-hardening characteristics.
3003 aluminum is an alloyed version of pure aluminum with the addition of Mangan (Bungbulang) (pangetan. 1.0-1,5%). This slight modification significantly boosts its tensile strength while maintaining the excellent formability of the 1000 runtuyan.
Studi kasus: Resolving Cracking Issues for a Middle Eastern Cookware Manufacturer
Last year, a large-scale cookware producer contacted Eco-Alum regarding their production of 25cm deep stock pots. They were experiencing a staggering 15% scrap rate due to cracking at the base.
Our Diagnosis: Metal-lographic analysis revealed an inconsistent grain size in their previous supply. During the second draw, the coarse grains caused localized thinning.
The Solution: We supplied Fine-Grain Annealed 3003-O temper circles. By controlling the cold reduction rate and recrystallization temperature, we ensured a grain size of ASTM 6 or finer.
The Result: Their scrap rate dropped from 15% ka 0.8%, saving the client thousands of dollars in monthly material costs.
2. Spésifikasi téknis: 3003 H14 Aluminum Properties
For engineers and procurement managers, the technical data is what matters most. Below is the physical property chart for 3003 H14, a widely used temper for moderate deep drawing and structural components.
3003 H14 Mechanical Properties Table
| Harta | Nilai (Metric) | Nilai (Imperial) |
| Kakuatan regangan | 145 – 185 MPa | 21 – 27 ksi |
| Kakuatan ngahasilkeun | 125 MPa (min) | 18 ksi (min) |
| Elongation di Break (50mm) | 8% – 12% | 8% – 12% |
| Teu karasa (Brinell) | 40 | 40 |
| Kapadetan | 2.73 g/cm³ | 0.0987 lb / ³³ |
| Konduktivitas termal | 193 W / m-k | 1340 BTU-in/hr-ft²-°F |
Catetan: For extreme deep drawing (ratios > 2.0), éta “O” (diantared) temper is recommended to maximize elongation (nepi ka 25% atawa leuwih).

3. Deep Drawing Comparison: 3003 vs. 1100 alumunium
A common question among buyers is: “Can I just use 1100 aluminum since it’s cheaper and softer?” Sedengkeun 1100 is highly formable, it often fails in industrial applications like cookware for two critical reasons:
A. Kakuatan sareng daya tahan
3003 nyaéta kira-kira 20% notuna kuat kuat ti 1100. In a pressure vessel, this allows for thinner walls without sacrificing safety. Cookware made from 3003 is far more resistant to warping and denting during daily use.
B. The “Orange Peel” Pangaruhna
When 1100 aluminum is stretched heavily, the grains can slide unevenly, creating a rough surface known as “orange peel.”
Technical Insight: The Manganese in 3003 creates “dispersoids” that pin grain boundaries. At our factory, we’ve measured that 3003 surfaces after drawing are 40% smoother (lower Ra value) ti 1100, which reduces the time and cost needed for final polishing.
4. Aplikasi Hual: From Kitchens to EV Batteries
EV Battery Shells (The 2026 Trend)
The electric vehicle revolution has seen a surge in demand for 3003 alumunium.
Real-World Case: A battery component supplier faced issues with “cinyusu” (deformation after the punch is removed), leading to welding failures on battery lids.
Our Expert Fix: We implemented Batch-Level Consistency Control. By ensuring every coil had a hardness variation of less than ±2 HV, we stabilized the springback rate, allowing their automated laser welding lines to run 24/7 without adjustment.
Other Key Applications:
-
Sistem HVAC: 3003 is the standard for evaporator coils due to its corrosion resistance.
-
Fuel Tanks: Excellent weldability ensures leak-proof seams under vibration.
-
Semi-Rigid Containers: (For thinner gauges, our sister site [aluminumfoilroll.com] provides specialized 3003 foils for food containers).

5. Pro Tips for Successful 3003 Ngagambar Jero
Drawing 3003 isn’t just about the metal; it’s about the process. Here are three expert tips from our technical department:
-
Select the Right Lubricant: Never use standard machine oil. Use a water-soluble drawing oil with Extreme Pressure (EP) additives. This prevents “galling” (metal transfer) between the 3003 sheet and the die.
-
Blank Holder Pressure: Margi 3003 is stronger than 1000 séri allah, it requires 15-20% higher pressure to prevent wrinkling without causing tears.
-
Die Clearance: Keur 3003, we recommend a die clearance of 1.1x to 1.15x the sheet thickness to accommodate the natural thickening of the alloy during the draw.

6. Patarosan anu sering ditaroskeun (FAQ)
Q: Geus 3003 aluminum food safe? A: Sumuhun. 3003 aluminum meets FDA and international food contact standards, making it the top choice for pots, paner, and food processing equipment.
Q: Tiasa 3003 be heat-treated to increase hardness? A: Henteu. 3003 is a non-heat-treatable alloy. Its strength is increased through cold working (galur gembleng).
Q: What is the maximum draw ratio for 3003-O? A: In ideal conditions with proper lubrication, 3003-O can achieve a draw ratio (Blank Diameter / Punch Diameter) of approximately 2.0 ka 2.2 in a single draw.
kacindekan: Partner with Eco-Alum for Your 3003 Supply
Success in deep drawing starts with the raw material. At Eco-Alum, we don’t just ship metal; we ship solutions. Urang 3003 Aluminum Sheets undergo rigorous testing—including Erichsen Cupping Tests jeung Spectrographic Analysis—to ensure that the material you receive performs perfectly on your press.
Get Your 3003 Aluminum Quote Today
Whether you are manufacturing EV components in Europe or cookware in Southeast Asia, Eco-Alum provides economical and efficient aluminum supplies with global shipping.
-
Official Website: https://eco-alum.com
Eco-Alum: Your Expert Partner for Professional Aluminum Solutions.